SustainedReleaseCoatingofDiclofenac
Pellets
1.Formulation
IPolymerSuspension:
KollicoatEMM30D[1]..........................224.1g IITalcSuspension:
Talc[10]...............................................29.3g Water.................................................228.8g to talI II:............................................482.2g SolidContentI II:.......................96.5g(=20%)
IIIDiclofenacsodiumspheronized
pellets30%(seeChapter5.4).................500g 2.Manufacturingofthesuspension
AddthetalcsuspensionIIto thewellstirredpolymersuspensionI.Stir
theobtainedsuspensionduringtheentirecoatingprocess.
3.Coatingprocedure,to pspray(FluidizedbedAeromaticStrea-1)
Loadingofdiclofenacpellets......................................................500g Quantityofspraysuspensionapplied.........................................482g Quantityofsolidsapplied............................................................97g Quantityofpolymerapplied.................................................4mg/cm2
Nozzle...................................................................................0.8mm
Sprayingpressure......................................................................1bar
Inlettemperature.......................................................................50C
Outlettemperature....................................................................33C
Airvolume.............................................................................80m3/h
Sprayrate............................................................................14g/min
Spraypressure........................................................................1.2bar
Spraytime...............................................................................35min
Dryingtime....................................................................5min(45C)
关键字:sustained release coating